Silicon Germainium wafers
2001-09-17
Kenneth Smith
2001-09-18
Tom Wester
Silicon Germainium wafers
Tom Wester
2001-09-18
Dear Ken,
ContactVirginia Semiconductor. They fabricate SiGe wafers and have
inventory you can view at
http://www.virginiasemi.com/products.cfm?cat=35

Regards,
Tom Wester

ProcessTek
PO Box 315
Lynnfield, MA 01940
office 781-595-1355, Fax 781-595-9582
[email protected]

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Kenneth Smith
Sent: Monday, September 17, 2001 8:54 PM
Cc: [email protected]
Subject: [mems-talk] Silicon Germainium wafers

This may not be the correct forum, but I have seen some involved in
Silicon Germanium respond here.
I am looking for a source of Silicon Germanium wafers in 3" diameter. I
can supply details specs if suppliers can be defined.

Best Regards,

Ken Smith
"when we were running for our lives, they ran the other direction to
attempt to save us"
http://www.Shark-Cove.com/CR/Code3.html

Kmbh Associates

4968 Charter Road
Rocklin, CA  95765  USA
510-714-5055 Efax- 510 217 4421 or 561 658 6136

High Purity Float Zone and Specialty CZ Silicon  for Power, IR and
Mirror Optics, Optoelectronics, MEMS, SOI, and other Semiconductor
applications. Service in SOI, Polishing SSP and DSP.

_______________________________________________
mems-talk mailing list
[email protected]
To unsubscribe or change your list options, use:
 http://fab.mems-exchange.org/mailman/listinfo/mems-talk



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics