I am currently bonding pyrex 7740 to Si wafers but the pyrex fluoresces too
much for my application.
Can anyone suggest a different kind of glass that can be anodically bonded
to Si wafers? As I understand it, the requirement is that the thermal
expansion coefficient of the glass matches that of silicon and that there
are ions available to migrate under the electric field across the interface.
Thanks!
Olgica

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
Mentor Graphics Corporation
Addison Engineering