MEMSnet Home: MEMS-Talk: photoresist bonding
photoresist bonding
2001-10-31
Jianzhong Zhu
2001-11-01
Jianzhong Zhu
2001-11-04
Luesebrink Helge
photoresist bonding
Luesebrink Helge
2001-11-04
Dear Jianzhong,

We are equipment manufacturer for the MEMS and microelectronics industry and
developed automated temporary bonding and debonding systems. Please feel
free to visit our Web site www.evgroup.com   or
contact us directly if you have any question regarding our systems.


Looking forward to hearing from you soon.
With very best regards,

Helge W. Luesebrink

EV Group US, Inc. - Regional Sales Manager -Tel: (401) 784 0008; Fax: (401)
784 9933; e-mail: [email protected] 
; Web site: www.EVGroup.com 





                -----Original Message-----
                From:   Jianzhong Zhu [mailto:[email protected]]
                Sent:   Wednesday, October 31, 2001 10:54 AM
                To:     [email protected]
                Subject:        [mems-talk] photoresist bonding

                Hi, All,

                Is there any body have experience to bond dry film
                photoresist onto silicon wafer? We hope to bond them
                directly, if possible.

                Thanks,
                Jianzhong
                Make a great connection at Yahoo! Personals.
                http://personals.yahoo.com
                _______________________________________________
                mems-talk mailing list
                [email protected]
                To unsubscribe or change your list options, use:
                 http://fab.mems-exchange.org/mailman/listinfo/mems-talk

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics