MEMSnet Home: MEMS-Talk: RE: mems-talk digest, Vol 1 #88 - 9 msgs - deposition of teflon
RE: mems-talk digest, Vol 1 #88 - 9 msgs - deposition of teflon
2001-11-10
Pancham R. Patel
RE: mems-talk digest, Vol 1 #88 - 9 msgs - deposition of teflon
Pancham R. Patel
2001-11-10
Dear Scott Goodwin-Johansson,

What thicknesses are you looking for?
If you require films in microns, Dupont sells amorphous fluoropolymers-
Teflon AF products.
You will have to use a flurosilane as an adhesion promoter.
Please do email me back if you want more information or
you may visit http://www.dupont.com/teflon/af/index.html

Thanks,
Pancham.
[email protected]

> From: Scott Goodwin-Johansson 
> To: "'[email protected]'" 
> Date: Thu, 8 Nov 2001 10:30:27 -0500
> Subject: [mems-talk] deposition of teflon
> Hi,
>       A colleague of mine has asked me about possible methods for
> depositing teflon on silicon.  If you have any experience or references I
> would appreciate hearing it.  Thanks in advance.
> Scott
> [email protected]

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Nano-Master, Inc.
MEMS Technology Review