MEMSnet Home: MEMS-Talk: Etch oxide not Aluminum?
Etch oxide not Aluminum?
2001-11-12
Yahong Yao
2001-11-12
[email protected]
2001-11-13
Roger Shile
Etch oxide not Aluminum?
Roger Shile
2001-11-13
You might try Olin 777 Etch.  Its NH4F , rather than HF based, and intended
for etching SiO2 over Al contact pads, without attacking the Al.

>>> "Yahong Yao"  11/12/01 09:47PM >>>
Hello Folks,

Is there any etchant which etches oxide fast but does not attack Al?
Thanks a lot.

Yahong

_________________________________________________________________
Get your FREE download of MSN Explorer at http://explorer.msn.com/intl.asp
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://fab.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Mentor Graphics Corporation
Harrick Plasma, Inc.