2001-12-07
Rajsekhar Popuri
2001-12-07
Michael Pedersen
2001-12-07
Rick Williston
2001-12-07
Bruno Wacogne
2001-12-10
Vladimir Gelfandbein
2001-12-07
[email protected]
lift-off
Rajsekhar Popuri
2001-12-07
Hello,

I am trying to do a lift-off.I sputter coated gold-palladium of 2000A
thickness on a glass wafer.When i tried to do a lift-off with
acetone-methanol,gold-palladium layer was completely peeled off the glass
wafer.Can anyone tell me the reason for this and suggest a suitable process
to do a lift-off with gold-palladium.

Thanks in advance
Rajsekhar.




_________________________________________________________________
Get your FREE download of MSN Explorer at http://explorer.msn.com/intl.asp

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
MEMS Technology Review
Process Variations in Microsystems Manufacturing