MEMSnet Home: MEMS-Talk: Re: SIMULATION TOOLS FOR ANISOTROPIC WET SILICON ETCHING
Re: SIMULATION TOOLS FOR ANISOTROPIC WET SILICON ETCHING
1996-06-19
[email protected]
1996-06-25
Erik K. Antonsson
Re: SIMULATION TOOLS FOR ANISOTROPIC WET SILICON ETCHING
[email protected]
1996-06-19
IntelliSense Corporation has a commercial software called ANISE for the
anisotropic etching of silicon. This software is part of the general purpose
CAD developed by IntelliSense, called IntelliCAD.

The price of the ANISE software is $3,995.00 and it runs on Unix workstations
with 50% discount for academic institutions. For further information please
contact:

IntelliSense Corporation
16 Upton Drive
Wilmington, MA 01887
(508) 988 - 8000 Tel
(508) 988 - 8001 Fax
[email protected] Email


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer