MEMSnet Home: MEMS-Talk: plasma chemistry for E-glass etching
plasma chemistry for E-glass etching
2001-12-07
Robert Dean
2001-12-07
martin.walker4
2001-12-07
[email protected]
2001-12-08
[email protected]
2001-12-11
Jon Doe
any hydrophillic layer?
2001-12-11
jung hoon yeom
2001-12-12
Helen Berney
2001-12-11
[email protected]
plasma chemistry for E-glass etching
[email protected]
2001-12-11
That would be too deep and too steep of an angle for us to be able to
recommend any tool that I know of now. Thanks for the input Bob Henderson

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
Nano-Master, Inc.
Addison Engineering