MEMSnet Home: MEMS-Talk: looking for PZT etchant
looking for PZT etchant
2001-12-11
[email protected]
2001-12-12
Gurvinderjit Singh
2001-12-13
Haigh, Richard Daniel
looking for PZT etchant
Gurvinderjit Singh
2001-12-12
Try Nitric acid (HNO3) 30% etching   time 3-4 minutes for ceramic, 5-7 min
for single crystal




On Wed, 12 Dec 2001 [email protected] wrote:

> hi,
>
> does anyone know the etchant for PZT?
> thanks in advance.
>
> Kun-lung Yen
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
MEMStaff Inc.
Process Variations in Microsystems Manufacturing