MEMSnet Home: MEMS-Talk: sticking
sticking
2001-12-13
jafar j babaei
2001-12-13
Paolo Bondavalli
2001-12-13
Helen Berney
sticking
Paolo Bondavalli
2001-12-13
Hi Jafar,
Supercrytical CO2 drying.
SCCO2
SC Fluids or Tousimis are the principal suppliers.
Bye

jafar j babaei a icrit :

> Hi all
>
> can anyone suggest an effective method to prevent sticking of released
> microstructures after rinsing?
>
> Thanks
> Jeff
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

--
**********************************************
Dr. Paolo Bondavalli
R&D Engineer
LABCOM - Laboratoire Interconnexions Optiques et MEMS
THALES (ex THOMSON-CSF) CORPORATE RESEARCH CENTER
Domaine de Corbeville,
Route Departementale 128
F91404 ORSAY
(FRANCE)
Tel : 01 69 33 08 63
Fax : 01 69 33 08 62
Email : [email protected]
**********************************************

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Addison Engineering