MEMSnet Home: MEMS-Talk: GaAs/Al(0.15)Ga(0.85)As selective etch
GaAs/Al(0.15)Ga(0.85)As selective etch
2001-12-13
Qingwei Mo
GaAs/Al(0.15)Ga(0.85)As selective etch
Qingwei Mo
2001-12-13
Hi, I am looking for some etchant of GaAs which can stop on
Al(0.15)Ga(0.85)As. Citric Acid and Hydragen Dioxide don't have enought
selectivity. I was told Amonium Hydraoxide and Hydragen Dioxide can do this
job, if I adjust it to right PH value. any clue about this problem? Or where
can I find the detail study about the Amonium etchant on GaAs/AlGaAs system.

Thanks a lot
Qingwei

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review
Process Variations in Microsystems Manufacturing