MEMSnet Home: MEMS-Talk: Re: thermal conductivity of polyimide?
Re: thermal conductivity of polyimide?
1996-06-26
Ladislav MATAY
1996-06-26
Mac McReynolds
Re: thermal conductivity of polyimide?
Ladislav MATAY
1996-06-26
Peter DOWSETT wrote:
>
> Hi,
>
> The title says it all.
>
> Does anybody know the thermal conductivity of polyimides in
> general and PIX3400 (from Hitachi) in particular?
>
> We have looked in the data sheets and found every number
> except this.
>
> Previous attempts at communication with Hitachi Japan seem to have
> failed due to language problems.
>
> Thank you, Peter Dowsett
> M. Eng. student, Micro Machines Research Group
> Electrical Engineering, RMIT
> Preferred e-mail address: [email protected]
> home page http://minyos.its.rmit.edu.au/~psd
>
Dear Peter,

there are data of thermal conductivity of polyimides:

    polyimide resin AURUM (Mitsui Toatsu Chemicals, Inc.)
    0.15 kcal/m.hr.C
    photosensitive polyimide Selectilux HTR3 (fy MERC)
    1600 J/cm.s.C
polyimide Probimide 200 Series (Ciba-Geigy Corp.)
    39x10exp(-5) cal/cm.s.C
    polyimide PYRALIN PI 2540, PI 2545 (Du Pont)
    37x10exp(-5) cal/cm.s.C

        PI 2550,2560,2562

    35x10exp(-5) cal/cm.s.C
    polyimide 7550 (Furane Products Co.)
    4x10exp(-4) cal/cm.s.C
polyimide PIQ 13 (Hitachi)
    4x10exp(-4) cal/cm.s.C

Sincerely yours
Ladislav
--
LADISLAV MATAY
INSTITUTE OF COMPUTER SYSTEMS
SLOVAK ACADEMY OF SCIENCES
SK-84237 BRATISLAVA
SLOVAKIA
TEL: 0042.7.3782743
FAX: 0042.7.371004
[email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
The Branford Group