MEMSnet Home: MEMS-Talk: Hard mask for 20 um deep SiO2 RIE etch?
Suppliers for Diamond Drill Bits?
2001-12-19
Jordan M. Berg
Hard mask for 20 um deep SiO2 RIE etch?
2001-12-19
Jon Doe
2001-12-19
X. Yuan
2001-12-21
Jon Doe
Thick positiv resist
2001-12-21
Jon Doe
LTO in a Novellus reactor?
2001-12-19
Jon Doe
2001-12-19
Vic Kley
2001-12-19
Jim Intrater -- IE
Hard mask for 20 um deep SiO2 RIE etch?
X. Yuan
2001-12-19
Hi, have you ever tried just thick PR?
I am not sure about your specific
etching conditions. Just a suggestion.
By the way, is there any special equipment
that can do such a thick SiO2 etch?

Thanks a lot.

Yuan
Check out Yahoo! Shopping and Yahoo! Auctions for all of
your unique holiday gifts! Buy at http://shopping.yahoo.com
or bid at http://auctions.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Addison Engineering
Process Variations in Microsystems Manufacturing