A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Does anyone know where I should look for ceramic test coatingservices?
Does anyone know where I should look for ceramic test coatingservices?
2002-01-15
Walter Stonas
2002-01-15
Vladimir Gelfandbein
Does anyone know where I should look for ceramic test coatingservices?
Vladimir Gelfandbein
2002-01-15
Hi Lisa,

We are doing all this in cooperation with  the  Berkley Lab/LBNL.

Dr. Vladimir Gelfandbein
Nayna Networks
481 Sycamore Drive
Milpitas, CA 95305
Ph.408- 956 8000 ( 449)


-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of Walter Stonas
Sent: Tuesday, January 15, 2002 10:02 AM
To: [email protected]
Subject: RE: [mems-talk] Does anyone know where I should look for
ceramic test coatingservices?


Hi Lisa,

Have you tried Scientific Coating Inc in San Jose.(408)-727-3296.

Sincerely,
Walter Stonas



-----Original Message-----
From: Lisa Stringo [mailto:[email protected]]
Sent: Monday, January 14, 2002 4:36 PM
To: [email protected]
Subject: [mems-talk] Does anyone know where I should look for ceramic
test coatingservices?


Does anyone know where I can find the following coating services for ceramic
test wafers 1 x 1 1/2 and 2 x 2 1/2?

-Titanium Dioxide Deposition
-Sputtered deposition
-cathotic arch deposition

Can you control the resisitivity of the titanium dioxide on a ceramic test
wafer?

Thank you for your time.

Lisa Stringo
Account Manager
Silicon Valley Microelectronics, Inc.
Tel: 408-985-5139
Fax: 408-244-6075
Email: [email protected]
http://www.svmi.com
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Harrick Plasma, Inc.
Mentor Graphics Corporation