A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: KOH etch
KOH etch
2002-01-18
Ryan Hickey
2002-01-18
Roger Shile
2002-01-18
Roger Brennan
KOH etch
Roger Brennan
2002-01-18
"I have heard that Chrome will hold up well to KOH."

Check out this URL:

http://galaxy.micro.uiuc.edu/facilities/processes/etching/silicon_cr_in_koh.html

-----Original Message-----
From:   Roger Shile [SMTP:[email protected]]
Sent:   Friday, January 18, 2002 9:34 AM
To:     [email protected]
Subject:        Re: [mems-talk] KOH etch

LPCVD silicon nitride is commonly used as a mask for KOH etching silicon,
though SiO2 may suffice if its thick enough.  I find 30w% KOH to etch thermal
SiO2 at ~20 angstroms/min at 80 degC, while etching Si at ~1 micron/min.  CVD
films will probably etch faster.

I have heard that Chrome will hold up well to KOH.

>>> [email protected] 01/18/02 06:58AM >>>
Hi All,

I'm going to do a deep 10 hour KOH etch of Silicon and am wondering what the
best mask is and how it should be applied.  What are the advantages and
disadvantages?  Residual stresses; Porosity; Temperature; Recomended
thickness; Deposition (LPCVD, PECVD); Thermal

SiO2?
SiN?
PSG?
etc...

Thank you

Ryan
[email protected]



_________________________________________________________________
Send and receive Hotmail on your mobile device: http://mobile.msn.com
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
The Branford Group
Process Variations in Microsystems Manufacturing