MEMSnet Home: MEMS-Talk: wet etchant of Silicon with etch rate in few nm/min
wet etchant of Silicon with etch rate in few nm/min
2002-01-23
Mohammed Javeed Shaikh
wet etchant of Silicon with etch rate in few nm/min
2002-01-24
Bernard Legrand
Need to remove a couple of thin layers from a GaAs wafer
2002-01-29
Xinbing Liu
wet etchant of Silicon with etch rate in few nm/min
Mohammed Javeed Shaikh
2002-01-23
hello everyone,
    can any one help me with wet etching of silicon. the etchant should etch
apprx at nm/min. For the etchant, positive Photoresist should act as mask.

thank you,
Javeed Shaikh Mohammed




-------------------------------------------------
This mail sent through IMP: http://horde.org/imp/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing