MEMSnet Home: MEMS-Talk: AW: negative photoresist.
AW: negative photoresist.
2002-01-30
Bruckner, Miriam
AW: negative photoresist.
Bruckner, Miriam
2002-01-30
Hi Peng,
the negative resist Durimide 7000 can be removed easily by NMP.
Also it is not too sensitive to N2.
Good luck
Miriam




Message: 3
From: "Peng Jin" 
To: 
Date: Tue, 29 Jan 2002 10:33:58 -0000
Subject: [mems-talk] Negative Photoresist
Reply-To: [email protected]

Hi, friends,

In my research project, I need to find a kind of negative photoresist which
must be easy to remove by acetone or other chemical solvent. Could anyone
give
me some idea about it?

Thanks.

Peng Jin

--__--__--

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.