MEMSnet Home: MEMS-Talk: Information/Paper reference about wet silicon nitride etchant.
Information/Paper reference about wet silicon nitride etchant.
2002-02-04
[email protected]
Information/Paper reference about wet silicon nitride etchant.
[email protected]
2002-02-04
By far the best method for etching Nitride is plasma. It provides control of
undercut and it doesn't require hot phosphoric acid.

reply
Events