Thick SOI wafers
2002-02-11
Luesebrink Helge
2002-02-11
Lawlor, Chris
Thick SOI wafers
Lawlor, Chris
2002-02-11
Hi Alok,
We offer SOI wafers with thickness 2um - 100+ um.
Oxides 0.2-3um as standard.
Website is www.bco-technologies.com , we are now part of Analog Devices.
 You can contact me directly if you have any queries.
#######
Apologies to those with no interest in SOI, sorry for taking up email space
!

Chris..


-----Original Message-----
From: Alok Paranjpye [mailto:[email protected]]
Sent: 11 February 2002 05:41
To: [email protected]
Subject: [mems-talk] Thick SOI wafers


Hi Everyone,
I'm looking for bonded SOI wafers with a thick (10um+) top Si layer and 2-3
um BOX layer. I haven't been able to find any vendor that makes such thick
Si layers. I'd be grateful for any leads on this, or if somebody could tell
me what is the thickest Si layer available out there.
Thanks!!
Alok Paranjpye
Graduate Student Researcher
Mechanical & Environmental Engg.
University of California
Santa Barbara 93016
Ph:  805-893-5341
Fax: 805-893-8651
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review
Process Variations in Microsystems Manufacturing