A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Positive resists for MEMS processing
Positive resists for MEMS processing
2002-02-18
[email protected]
2002-02-18
C. Suzanne Miller
Making metal clusters on Si substrate
2002-02-19
Junghoon Yeom
2002-02-18
Rohit Srivastava
2002-02-18
Jon Doe
2002-02-19
Liz Shelley
2002-02-19
Blunier, Stefan
2002-02-19
[email protected]
2002-02-19
[email protected]
2002-02-19
[email protected]
Positive resists for MEMS processing
[email protected]
2002-02-19
Thomas:
Would you have the capability to process 10 wafers with this resist and apply
a photomask of MEMS trenches from 2-50 microns. We will gladly pay for the
samples. This will allow us to evaluate this resist for deep silicon etches.
Bob Henderson 480-558-1156

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Harrick Plasma, Inc.
Mentor Graphics Corporation