MEMSnet Home: MEMS-Talk: looking for SOI wafers with thick Oxide layer
looking for SOI wafers with thick Oxide layer
2002-02-27
Oberhammer Joachim
2002-02-27
Lawlor, Chris
looking for SOI wafers with thick Oxide layer
Lawlor, Chris
2002-02-27
Hi Joachim,
I have some wafers from our stock range which match your requirements fairly
closely.
Just drop me an email and we can discuss further.

Best wishes,
Chris Lawlor
Analog Devices Belfast.



-----Original Message-----
From: Oberhammer Joachim [mailto:[email protected]]
Sent: 27 February 2002 15:32
To: [email protected]
Subject: [mems-talk] looking for SOI wafers with thick Oxide layer


I'm looking for supplier of SOI wafers fulfilling the following
(major) specifications:
- 100 mm diameter
- oxide layer thickness > 2.5 um (preferred up to 4 um)
- Si top layer 8-20 um thick (preferred: 10 um)
- low volume: about 5 pieces

If you have such wafers on the stock and would like to get rid of
them, or you know any supplier, please come back to me. Thanks.
--
-----------------------------------------------------------------------------
-
Joachim Oberhammer, Dipl.-Ing.

Royal Institute of Technology (KTH)   Phone:    +46/(0)8 790 6250
Dep. of Signals, Sensors and Systems  Fax:      +46/(0)8 10 0858
Microsystem Technology (MST)          Mobile:   +46/(0)70 692 1858
                                       e-mail:   [email protected]
Osquldas vdg 10                       homepage: http://www.s3.kth.se/mst/
SE-100 44 Stockholm, Sweden
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation