MEMSnet Home: MEMS-Talk: Plating on stainles steel
Plating on stainles steel
2002-03-21
Liz Shelley
2002-03-22
Abhinav Bhushan
2002-03-21
BERAUER,FRANK (HP-Singapore,ex7)
2002-03-22
John Somerville
Plating on stainles steel
John Somerville
2002-03-22
tecan.co.uk

have helped us with this previously they have a process for generating a
nickel seed layer which will attach.

I'm sure they are others if you are in the US

John

reply