A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: photosensitive polyimides
photosensitive polyimides
2002-03-28
Balaji Lakshminarayanan
2002-03-28
Liz Shelley
2002-04-01
Inna
2002-03-28
Mac McReynolds
2002-03-28
[email protected]
2002-04-03
Rivas, Isabel
photosensitive polyimides
Inna
2002-04-01
Hi Bala,

There are two more companies that I know of.

Dow Chemicals at www.dow.com. They have photosensitive polyimide Cyclotene.
You  can visit their web site at www.cyclotene.com

Another company is HD Microsystems (Hitachi + DuPont joint) at
www.hdmicrosystems.com

Good luck,


Inna Mushkatinskaya

Sr. Process Specialist
Anvik Corporation
6 Skyline Drive
Hawthorne NY 10532

Tel: 914-345-2442, etx.18
Fax: 914-345-2452

Web: www.anvik.com
E-mail: [email protected]


on 3/28/02 12:02 AM, Balaji Lakshminarayanan at [email protected] wrote:

> Hi,
>
> Can anyone tell me companies that sell photosensitive polyimides. I am
> using it as a dielectric for variable capacitors. I searched the web and
> found clariant (their PIMEL series) sells the same, but they told us the
> quantities they ideally sell is difficult for educational institution to
> handle.
>
> Your help is greatly appreciated
>
> regards
>
> bala
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Addison Engineering