Re: TI Etch for Silicon Defects (Non-Chromium)
2002-04-24
lib zhou
Re: TI Etch for Silicon Defects (Non-Chromium)
lib zhou
2002-04-24
Art:

you can etch Ti through RIE with the etchant gas CHF3, as the gasified by
fluorine atoms, which have high selective to silicon crystal at the same time.I
have do experience with good result, hope this useful to you!

Lib