Hallo Ralf,
I use Sylgard 184 and I use a thinner called Dow Corning Fluid 200 (20cSt).
I have made a ratio 1:3 and it works fine for my applikation - if you want
use more thinner than goes it to a gel.
Jens

----- Original Message -----
From: "Ralf A_mann" 
To: ; 
Sent: Thursday, April 25, 2002 12:09 PM
Subject: [mems-talk] pdms, spin coating


> Hi everybody!
> I want to coat some pmma with pdms by spin coating. Does anyone has some
> knowledge about this problem? The thickness must be about 55m. Is there
> an ideal viscosity and thinner I can use?
> Thanx and best regards!
>
> [demime 0.98e removed an attachment of type text/x-vcard which had a name
of Ralf.Assmann.vcf]
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
The Branford Group
Tanner EDA by Mentor Graphics