A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Au-Sn solder
Au-Sn solder
2002-05-08
adnan merhaba
2002-05-09
Phil
2002-05-13
Dr. Hermann Oppermann
Au-Sn solder
adnan merhaba
2002-05-08
hello all,

does anyone have any experiences with plating Au-Sn
(80-20) solder alloy, or any other viable means of
depositing the same (apart from screen-printing,
sputtering and evaporation), or is there any available
literature on the same.

I am looking to plate/deposit Au-Sn on pads of various
sizes ranging from 100x100 mils to 20x20 mils,
thickness ranging from 5 micron to 50 microns.

Thanking you in anticipation.
Regards,
Adnan
Yahoo! Health - your guide to health and wellness
http://health.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
University Wafer