MEMSnet Home: MEMS-Talk: PDMS pillar shape
PDMS pillar shape
2002-05-16
Bo He
2002-05-16
Bill Moffat
2002-05-17
mmf
2002-05-20
Bill Moffat
2002-05-20
mmf
PDMS pillar shape
Bill Moffat
2002-05-16
Bo,
   What size pillars and what material.  I have a paper on producing pillars
in Photoresist that are 0.5 microns diameter and 1.2 microns high.  Using
image reversal the angle of the side wall can be varied +/- 10 degrees from
vertical with ease  In the case of this paper the author wanted vertical side
walls.  Then flowing TEOS around the reversed image photo resist he defined
contacts with vertical side walls and increases the speed of his devices 40%
and decreased the size by 60%.  let me know if this process can help.  Bill
Muffed

-----Original Message-----
From: Bo He [mailto:[email protected]]
Sent: Thursday, May 16, 2002 9:50 AM
To: [email protected]
Subject: [mems-talk] PDMS pillar shape


Dear All:

         I am working on making pillar arrays by PDMS. But when I pull
out PDMS from SU8 mold, I found most pillars were deformed (bent). The
reason I am thinking about is that the cavity on SU8 mold has positive
slope hence PDMS pillar has negative slope. The the top of PDMS pillar,
which is in contact with the bottom of the cavity on SU8 mold, is larger
then the bottom, so it's deformed or bent during pulling out. Is there
anyway to solve the problem? Any suggestion is highly appreciated.

Bo

------------------------------------------------------------------------

Chat with friends online, try MSN Messenger: Click Here
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Addison Engineering