Ash Parameswaran
1996-02-22
[email protected]
Re: Diaphragms via Wafer Bonding
Ash Parameswaran
1996-02-10
If you dope it with Boron, then it inrodues some tensile stress and it might
help stretch the thin membrane.

This technique is used by many US EPI/Etch-Stop wafer manufacturers for MEMS
applications.