A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: TMAH effetc on Chromium and Polyimide film
TMAH effetc on Chromium and Polyimide film
2002-06-02
aslam muhammad
2002-06-06
shay kaplan
2002-06-12
Sandra Bermejo
TMAH effetc on Chromium and Polyimide film
shay kaplan
2002-06-06
Aslam,
THe films aren't attacked but will many times be undercut - depending on
the substrate and deposition process.

Shay

aslam muhammad wrote:

> Hi everbody
>  I need a small information as experts openion plz.
>
> What is the effect of TMAH 25% at 80-90C on chromium
> layer and on polyimide membrane ( cured at 350 c).
>
> Needs ur experienced openion.
>
> Good luck for all
>
> M. Aslam
> Yahoo! - Official partner of 2002 FIFA World Cup
> http://fifaworldcup.yahoo.com
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics