MEMSnet Home: MEMS-Talk: re etching cavities in borosilicate glass
re etching cavities in borosilicate glass
2002-06-28
Richard Morrison
re etching cavities in borosilicate glass
Richard Morrison
2002-06-28
hi,

You can try to contact Bullen Ultrasonics , tel  513-456-7133. The
ultrasonically mill glass. They do very nice work.

Rick


Rick Morrison
Sr. Semiconductor Engineer
Radant Mems Inc.
255 Hudson Road
Stow Ma, 01775
Tel- 978-562-3866
Cell 508-801-4796
AMS Phone: 508-770-3521
EMAIL  [email protected]

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Harrick Plasma, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing