2002-07-09
Dear Bill
I'm not sure that the dn/dt coefficient could be correlated to the amount of
oxygen present during the curing
Could you provide me some references about that phenomena.
I'm interested in any kind of polymers , possibly UV curable.
Best Regards

Mario

-----Messaggio originale-----
Da: [email protected] [mailto:[email protected]]Per
conto di Bill Moffat
Inviato: lunedl 8 luglio 2002 20.15
A: [email protected]
Oggetto: RE: [mems-talk] thermo optic polymers


Mario,
       What do you mean polymers thermo optic measurement?  The rate of
change
of the refractive
index with temperature?  This can change dependent upon the amount of oxygen
present when the polymer is cured.  Let me know what type of polymer and
what
type of curing.  Bill Moffat
-----Original Message-----
From: cortese [mailto:[email protected]]
Sent: Monday, July 08, 2002 10:42 AM
To: [email protected]
Subject: [mems-talk] thermo optic polymers


Dear All
I'm interested in polymer's thermo optic measurement.In particular I would
like to know what kind of instruments could be used for it.
Any suggestion would be appreciate.
Thanks
Mario
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
The Branford Group