MEMSnet Home: MEMS-Talk: tantalum processing questions
tantalum processing questions
2002-07-15
Muralidhar K. Ghantasala
2002-07-16
TEL Klaus Beschorner
tantalum processing questions
TEL Klaus Beschorner
2002-07-16
> We are considering the use of Ta for simple coplanar electrode strips (10
> microns wide and 1000 microns long) patterned on quartz wafers, or maybe on
> top of an LTO layer deposited on the quartz.  I imagine we have to
> planarize to put this stuff down on the LTO, but are adhesion promoters
> needed?  Are there any serious pitfalls to avoid in the use of this metal?

Thomas,
there's lots of details, as usual, which depend on the deposition method
you consider. I assume that for an electrode application, film
resistivity will be an issue. alpha- and beta-Ta have widely different
Rs, substrate temperature is the main controlling parameter. You don't
want to work in a region where you deposit a mixture of both phases.

best regards,
klaus
--

                        (TEEL)          Tokyo Electron Europe Limited
                                        PVD Process Support  (ex MRC)
Klaus Beschorner                                   Tel +49-7033-45683
Drosselweg 6                                       Fax +49-7033-45631
71120 Grafenau, Germany                       Mobile +49-174 315 7754

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Tanner EDA by Mentor Graphics
University Wafer