MEMSnet Home: MEMS-Talk: charges
charges
1996-10-23
John Sidles
charges
John Sidles
1996-10-23
We too see charges accumulate on SiN cantilevers.
We neutralize them with a radioactive source,
which are cheaply available for this purpose.


reply