MEMSnet Home: MEMS-Talk: diametmer 100um-300um silica sphere
diametmer 100um-300um silica sphere
2002-07-26
Dlee Li
2002-07-29
Anwei Qin
diametmer 100um-300um silica sphere
Anwei Qin
2002-07-29
MO-SCI has micro glass spheres of different sizes and compositions. You
may contact Gary Brand (573-364 0300) for more information.

Anwei Qin

Dlee Li wrote:

> hi, friend
> Anyone can tell me where i can buy diametmer 100um-300um silica sphere?
> Any information will be appreciated. T
>
> Thanks
> dlee
> Research Assistant
> Mechanical Engineering Department
> the University of Texas At Austin
>
> _________________________________________________________________
> Send and receive Hotmail on your mobile device: http://mobile.msn.com
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.