MEMSnet Home: MEMS-Talk: Recipe for SU-8 2100
Recipe for SU-8 2100
2002-08-05
#TRUONG THAI QUANG#
Recipe for SU-8 2100
#TRUONG THAI QUANG#
2002-08-05
Hi,

I am using SU-8 2100 (Microchem) to form structure with thickness of 100 um.
However, I could not find the correct recipe for SU-8 2100 from Microchem
website. I tried to use the recipe of SU-8 100 but could not get the correct
thickness.

Has any one successfully used SU-8 2100 to achieve uniform 100um layer ?

Thanks

Quang
Nanyang Technological University, Singapore

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Mentor Graphics Corporation
Addison Engineering