MEMSnet Home: MEMS-Talk: Shear stress from polishing
Shear stress from polishing
2002-08-08
Haigh, Richard
Shear stress from polishing
Haigh, Richard
2002-08-08
Dear collegues

I intend to bond a ceramic disk to a buried oxide wafer, and then polish
the disk to the desired thickness. Is anyone aware of difficulties
associated with the shear stresses that might be generated during
polshing? Is it possible for the polishing process to damage the thin Si
layer above the buried oxide layer?


Regards



Richard Haigh

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMStaff Inc.
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing