MEMSnet Home: MEMS-Talk: Patternable PDMS
Patternable PDMS
2002-08-19
Bo He
2002-08-20
Suzanne M. Snyder
2002-08-22
allen kine
Patternable PDMS
Bo He
2002-08-19
Dear MEMS expert:

        Are there any articles about how to pattern PDMS by conventional
photolithography? Any input is highly appreciated.



Bo



------------------------------------------------------------------------

Join the worlds largest e-mail service with MSN Hotmail. Click Here