MEMSnet Home: MEMS-Talk: Laser printer masks
Laser printer masks
2002-08-20
Michael Wulf
2002-08-21
weiwei
2002-08-21
David Nemeth
2002-08-21
BERAUER,FRANK (HP-Singapore,ex7)
Laser printer masks
Michael Wulf
2002-08-20
Hi,

i need some cheap masks; the easiest solution we found is using a
laser-printer on overhead foiles. the structure size i can reach with this
is so far limited to be 200microns.

does anybody have experinece how to make structures smaller (without
spending money on a mask) and what brands (models) of transparencies and
printers might be good ? (i aim at a factor of 2 to 4 in structure size)

does anybody know a place where you can buy such really cheap masks with
even better resolution ?


thanks already,

mike

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
The Branford Group
Tanner EDA by Mentor Graphics