Cleaning Germainium Wafers
2002-08-19
Maurice Norcott
2002-08-29
Attenborough, Karen
Cleaning Germainium Wafers
Attenborough, Karen
2002-08-29
Hi Maurice

Sorry I don't know the answer to that one.

I have never mixed the two processes.

Best wishes

Karen



-----Original Message-----
From: Maurice Norcott [mailto:[email protected]]
Sent: 19 August 2002 21:00
To: '[email protected]'
Subject: RE: [mems-talk] Cleaning Germainium Wafers


Hi Karen,

Do you know if a silicon process & a Ge process can be run
through the same wetbench without cross-contamination ?

Thanks, Maurice

Maurice H. Norcott
Senior R&D Technician
Silicon Genesis Corporation
590 Division Street
Campbell, CA 95008
408-228-5847
Pager 408-977-6333





-----Original Message-----
From: Attenborough, Karen [mailto:[email protected]]
Sent: Thursday, August 01, 2002 7:29 AM
To: '[email protected]'
Subject: RE: [mems-talk] Cleaning Germainium Wafers


Hi Maurice

In the past, I have used Ge and used the following process steps to clean
it.

        rinse in cold and hot Acetone, followed by cold and hot IPA
        dip 1 min. in 10% NH4OH:H2O
        rinse at least 10 min. in DI-water
blow dry with special care because Germanium is hydrophilic

I only used small pieces of wafer, so the above process may not be perfectly
compatible with what you are using.

Hope this helps
With best wishes

Karen Attenborough


Dr. Karen Attenborough
OnStream MST  B.V.
Lodewijkstraat 1
5652 AC Eindhoven
The Netherlands
Tel:  +31.40.295.9814
Fax: +31.40.295.9906
Email: [email protected]
www.onstreammst.com



-----Original Message-----
From: Maurice Norcott [mailto:[email protected]]
Sent: 01 August 2002 04:02
To: '[email protected]'
Subject: [mems-talk] Cleaning Germainium Wafers


Sorry, I should have been more specific. I have a wafer cleaning sink
with megasonics etc. What I am looking for is recommended chemistries
to clean the Ge wafers in.


Maurice H. Norcott
Senior Technician
Silicon Genesis Corporation
590 Division Street
Campbell, CA 95008

408-871-3948 Office
408-977-6333 Pager
[email protected]
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review