MEMSnet Home: MEMS-Talk: Nickel etchant
Nickel etchant
2002-09-09
Phaneendra Medida(fabbi)
2002-09-09
David Nemeth
2002-09-09
Neal Ricks
2002-09-10
David Nemeth
2002-09-09
Neal Ricks
2002-09-09
Kishan Gupta
2002-09-10
Neal Ricks
2002-09-10
Kishan Gupta
2002-09-10
Eric Sanjuan
polymer materials
2002-09-11
Adrian Stoian
Nickel etchant
Kishan Gupta
2002-09-10
You are right. I have confused the Au-5 Cyantek gold etchant for aqua
regia. Aqua regia in our labs etched Nickel at about 100 nm/min. The Au-5
Cyantek solution of KI + I2 did not etch the Nickel. I apologize for the
confusion.

-- Kishan

At 06:10 AM 9/10/2002 -0700, you wrote:

>Kishan,
>Can you provide a reference for this data?  Could you have this solution
>confused with 1 part HCl with 3 parts HNO3?  That is what most people
>refer to as aqua regia, and I believe that it does etch Nickel at an
>appreciable rate.
>Neal
>  Kishan Gupta wrote:Aqua Regia, (KI + I2), etched Nickel at approximately
> 100 nm/min in past
>experiments.
>
>-- Kishan Gupta
>EECS Undergraduate, U.C. Berkeley
>
>At 11:47 AM 9/9/2002 -0700, you wrote:
> >Does this solution (KI(Potassium iodide)+I2(Iodine)+Water) Etch Nickel?
> >
> >Fabbi.
> >_______________________________________________
> >[email protected] mailing list: to unsubscribe or change your list
> >options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> >Hosted by the MEMS Exchange, providers of MEMS processing services.
> >Visit us at http://www.memsnet.org/
>
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/
>
>
>---------------------------------
>Yahoo! - We Remember
>9-11: A tribute to the more than 3,000 lives
>lost_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Mentor Graphics Corporation
Addison Engineering