MEMSnet Home: MEMS-Talk: pyrex 7740 microscope slides?
pyrex 7740 microscope slides?
2002-09-10
Christopher Khoury
2002-09-11
bille@npphotonics (Bill Eaton)
2002-09-12
Kenneth Smith
pyrex 7740 microscope slides?
Kenneth Smith
2002-09-12
Depending on how many you might try one of the Pyrex or Glass processing
houses like -Mark Optics

emailto:[email protected]


Ken

Christopher Khoury wrote:

> Hello,
>
> does anyone have a vendor source on pyrex 7740 microscope slides (25 x
> 75 mm)
> of 0.5-1 mm thick? I can't seem to find any information at corning or
> the usual mailorder sources. Thanks -chris
>
> --
> C. Khoury         Nanosphere, Inc.
> Microsystems Engineer


Kmbh Associates
47 Rocket Circle
Rancho Cordova, CA 95742  U  S  A
510-714-5055 Efax- 510 217 4421 or 561 658 6136
High Purity Float Zone and Specialty CZ Silicon  for Power, IR and
Mirror Optics, Optoelectronics, MEMS, SOI, and other Semiconductor
applications.




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Addison Engineering
Process Variations in Microsystems Manufacturing