2002-09-16
Yan Cheng
2002-09-17
Renie Duvall
Cu on Si
Yan Cheng
2002-09-16
I am considering to sputter the Cu on Silicon, with the Cr as adhesion
layer. The silicon will be thermal oxided 100 nm at first.

With my knowledge, the adhesion of copper evaporated on silicon is very
poor. Sometimes even with Cr as the intermediate layer, there are some
problem either with the poor adhesion between the copper and the
chromium (with breaking vacuum to change the evaporation sources), or
with poor adhesion between the chromium and the silicon (without breakig
vacuum).

Did anyone have the experience that the thermal oxide layer would help
to the adhesion? Will there are any possible problems and suggestions
for the process which I prepare to do? Thank you.

Yan Cheng


University of Kassel
Email:  [email protected]



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
The Branford Group
University Wafer