MEMSnet Home: MEMS-Talk: Electroless Ni on Au
Electroless Ni on Au
2002-10-30
Peter & Judy Wright
2002-10-30
David Nemeth
2002-10-30
[email protected]
Electroless Ni on Au
David Nemeth
2002-10-30
You might try a very brief electroplate of nickel to put down a seed layer.

David Nemeth
Senior Process Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA
Ph: (703) 961-9573 x206
Fax:(703) 961-9576

-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of Peter & Judy Wright
Sent: Wednesday, October 30, 2002 12:36 AM
To: [email protected]
Subject: [mems-talk] Electroless Ni on Au


Is it possible to plate electroless Ni on Au? I have exposed gold pads, in
openings in a silicon nitride passivation layer, which I want to bump. I
would like to use Ni as the UBM and electroless deposition would save me a
photolithography step. If it is possible, what is the chemistry that is
required to catalyze the reaction and will the Ni film adhere well to the
Au?

Thanks for any help.
Peter Wright
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://www.memsnet.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
The Branford Group
Process Variations in Microsystems Manufacturing