Dr Kevin Walsh,

recently I read an article "photolithography on micromachined 3D surfaces using
electrodeposited photoresits" Sensors and Actuators A 51 1995 51-54.

This talks about deposition of photoresist upto 3 um in etched surfaces.

may be this would be helpful.