BRIAN DOUGLAS
RE: Glass-Glass Bonding
BRIAN DOUGLAS
2002-12-18
Helen,

  Suss MicroTec Inc. supplies Glass to Glass bonding solutions for upto 6"
wafers.  Check out our website at www.suss.com, or you can contact me directly,
I would be happy to run some samples for you.

 Regards,
Brian Douglas
[email protected]