MEMSnet Home: MEMS-Talk: PMMA bonding
PMMA bonding
2003-01-09
[email protected]
PMMA bonding
[email protected]
2003-01-09
Hi all,

I am doing micromachining of microchannels on PMMA piece.  I am wondering if
somebody can tell me how to bond the PMMA to another piece of PMMA or onto
galss slide without damaging the microchannels?  Thanks alot!

Zhiyu


reply