MEMSnet Home: MEMS-Talk: Photo-definable glass
Photo-definable glass
2003-01-24
Sarah Schwab
2003-01-27
Karl Cazzini
2003-01-27
Mac McReynolds
2003-01-28
St.Clair, Loren
2003-01-28
Charles Ellis
2003-01-30
Paolo Bondavalli
2003-01-28
Bill Moffat
2003-01-30
St.Clair, Loren
Photo-definable glass
Sarah Schwab
2003-01-24
Hello there
I am looking for some information on photo-definable glass.
Could anyone please help me with the following:

Suppliers?
Approx cost per wafer 4" diameter - sample quantities?
Minimum thickness?

Many thanks
Sarah


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
The Branford Group
Process Variations in Microsystems Manufacturing