MEMSnet Home: MEMS-Talk: Silanisation
Silanisation
2003-02-12
Christabel Tan
2003-02-12
Alik Widge
2003-02-12
Bill Moffat
Silanisation
Christabel Tan
2003-02-12
Hi,

Does anybody know if SU-8 would withstand octadecyltrichlorosilane?

Christabel Tan
STRC
University of Hertfordshire
College Lane, Hatfield
Hertfordshire, AL 10 9AB
Email: [email protected]
Tel: 01707 284169
reply