Hi,

I was wondering if someone can tell  me the conditions required to grown
right crystal structure of  a Piezoelectric material namely AlN. Also some
equipment/method to sense the voltage in the range of 900 V.

Thanks for your time
Regards,
Priyanka

----- Original Message -----
From: "Vincent Mortet" 
To: 
Sent: Thursday, October 24, 2002 11:48 PM
Subject: RE: [mems-talk] Piezoelectricity Measurement


> Hi,
>
> I've not experience with this configuration. However I 'd like to prepare
> such cantilever with a piezoelectric layer and electrodes to measure the
> d31. According to me, you should have a look on refs // E Cattan et al,
> Sensors and Actuators 74 (1999) 60 and // B Jaber et al, Sensors and
> Actuators A 63 (1997) 91, were a measurment of e31 with a cantilever is
> described.
>
> Best regards,
> Vincent Mortet
>
> -----Original Message-----
> From: [email protected] [mailto:[email protected]]On
> Behalf Of Priyanka Aggarwal
> Sent: donderdag 24 oktober 2002 19:12
> To: [email protected]
> Subject: Re: [mems-talk] Piezoelectricity Measurement
>
>
> Hi,
> I am also working on the same lines. I was wondering where should I have
the
> metal contacts,I want to have them on the fixed end of the cantilever ,
but
> I am not sure how to make metal contacts till that surface. CAn you
suggest
> something.I am attching a document to make it clearer.
> Thanks
> Priyanka
>
>
>
>
>
> ----- Original Message -----
> From: "Vincent Mortet" 
> To: 
> Sent: Thursday, October 24, 2002 2:59 AM
> Subject: RE: [mems-talk] Piezoelectricity Measurement
>
>
> > Hello,
> >
> > 1/To measure the reverse piezoelectric coeffience d33 of "a layer" you
> have
> > to make a sandwich of it, between two elctectods on a thick substrate
> (2mm)
> > you can apply a AC voltage (frequency f0) to the layer and you measure
the
> > displasment of the top surface with a calibrated AFM or interferometer.
> For
> > the AFM method, you have to use the A-B signal from the photodetector
with
> > the frequency f0, ie filtered with an lock-in amplifier.
> >
> > 2/It exists a methode to measure the direct piezoelectric coefficient
e31
> > on which you collect the charges created by the piezo on the electrode
> > during the vibration on a cantilever covered with the piezoelectric
> > material.
> >
> > Here are some refs to help you on points  1/ A-L Kholin et al. Rev Sci
> > Instrum Vol 67 No 5 May 1996 1935
> > M-A Dubois et al, Appl Phys Lett,  Vol 89, No 11 (2001) 6389
> > C-M Lueng et al J Appl Phys, Vol 88, No 9 (2000) 5360
> > J-A Christman et al App Phys Lett, Vol73, No 26 (1998) 3851
> >
> > 2/ E Cattan et al, Sensors and Actuators 74 (1999) 60
> > B Jaber et al, Sensors and Actuators A 63 (1997) 91
> > J-F Shepard Jr et al, Sensors and Actuators A 71 (1998) 133
> >
> > Best regards,
> > Vincent Mortet
> >
> > -----Original Message-----
> > From: [email protected] [mailto:[email protected]]On
> > Behalf Of Xiaoqin Huang
> > Sent: woensdag 23 oktober 2002 19:56
> > To: [email protected]
> > Subject: [mems-talk] Piezoelectricity Measurement
> >
> >
> > Hi all,
> >
> > I am planning to measure the piezoelectricity of ZnO, but I just know a
> > bit about this kind of measurement. If you are familiar with this
> > measurement, please give me some suggestions. Thank you very much.
> >
> > Jenny X. Huang
> >
> >
> >
> > _______________________________________________
> > [email protected] mailing list: to unsubscribe or change your list
> > options, visit http://www.memsnet.org/mailman/listinfo/mems-talk
> > Hosted by the MEMS Exchange, providers of MEMS processing services.
> > Visit us at http://www.memsnet.org/
> >
> >
> > _______________________________________________
> > [email protected] mailing list: to unsubscribe or change your list
> > options, visit http://www.memsnet.org/mailman/listinfo/mems-talk
> > Hosted by the MEMS Exchange, providers of MEMS processing services.
> > Visit us at http://www.memsnet.org/
> >
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://www.memsnet.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Addison Engineering
Tanner EDA by Mentor Graphics