MEMSnet Home: MEMS-Talk: Re: Glow plasma color & leakage in a RF Sputtering
Re: Glow plasma color & leakage in a RF Sputtering
2003-02-20
Matteo Dainese
Re: Glow plasma color & leakage in a RF Sputtering
Matteo Dainese
2003-02-20
Pink is the color of the nitrogen plasma,
therefore you do have a leak.


reply